Re: Still massive stringing problems with my A20m
Posted: Wed Nov 04, 2020 7:53 pm
Old topic but here are some very interresting informations.
Retraction on mixing extruder just do not work as expected, and this is the key of stringing problems.
Basically when one side/filament is retracted, it suck from the other side/filament rather than from the nozzle , that's why the retraction just does not have any effect...
Here are some more informations
https://github.com/MarlinFirmware/Marlin/pull/11941
I found a solution that mitigate the problem when printing with one PLA filament I just use a higher temperature filament in the second extruder (ABS for example)
Here is Marlin 2 Configuration_adv.h settings you have to change to enable extruders synchronized retraction and completely remove stringing problems
Important : after flashing your firmware, you must send gcode M209 S1 to enable FWRETRACT_AUTORETRACT(this will enable conversion of your G1 E to firmware retract/unretract gcode while printing)
Hope it helps !!!
@admin : maybe this post should be stick as I have not seen around a lot of right answers (exept commons : lower your temp, increase your retract etc...) for stringing problems on mix extruder printer
Retraction on mixing extruder just do not work as expected, and this is the key of stringing problems.
Basically when one side/filament is retracted, it suck from the other side/filament rather than from the nozzle , that's why the retraction just does not have any effect...
Here are some more informations
https://github.com/MarlinFirmware/Marlin/pull/11941
I found a solution that mitigate the problem when printing with one PLA filament I just use a higher temperature filament in the second extruder (ABS for example)
Here is Marlin 2 Configuration_adv.h settings you have to change to enable extruders synchronized retraction and completely remove stringing problems
Code: Select all
#define FWRETRACT
#if ENABLED(FWRETRACT)
#define FWRETRACT_AUTORETRACT // Override slicer retractions
#if ENABLED(FWRETRACT_AUTORETRACT)
#define MIN_AUTORETRACT 0.1 // (mm) Don't convert E moves under this length
#define MAX_AUTORETRACT 15.0 // (mm) Don't convert E moves over this length
#endif
#define RETRACT_LENGTH 5 // (mm) Default retract length (positive value)
#define RETRACT_LENGTH_SWAP 13 // (mm) Default swap retract length (positive value)
#define RETRACT_FEEDRATE 45 // (mm/s) Default feedrate for retracting
#define RETRACT_ZRAISE 0 // (mm) Default retract Z-raise
#define RETRACT_RECOVER_LENGTH 0 // (mm) Default additional recover length (added to retract length on recover)
#define RETRACT_RECOVER_LENGTH_SWAP 0 // (mm) Default additional swap recover length (added to retract length on recover from toolchange)
#define RETRACT_RECOVER_FEEDRATE 8 // (mm/s) Default feedrate for recovering from retraction
#define RETRACT_RECOVER_FEEDRATE_SWAP 8 // (mm/s) Default feedrate for recovering from swap retraction
#if ENABLED(MIXING_EXTRUDER)
#define RETRACT_SYNC_MIXING // Retract and restore all mixing steppers simultaneously
#endif
#endif
Hope it helps !!!